Fiat Chrysler Automobiles NV is preparing to recall about 18,000 Jeep Wranglers because of a faulty weld in the frame of the popular sport utility vehicle that can cause a sudden crash.
The automaker will begin the recall before the end of the year, according to a dealer notice posted Friday on a Wrangler owner forum that was confirmed by the company. Some vehicles have a faulty weld on the front track bar, which keeps the axles centered. That can allow the bar to separate from the frame and interfere with the steering, “which can cause a vehicle crash without prior warning,” according to the notice.
https://www.bloomberg.com/news/arti...o-recall-new-wranglers-over-frame-weld-defect
				
			The automaker will begin the recall before the end of the year, according to a dealer notice posted Friday on a Wrangler owner forum that was confirmed by the company. Some vehicles have a faulty weld on the front track bar, which keeps the axles centered. That can allow the bar to separate from the frame and interfere with the steering, “which can cause a vehicle crash without prior warning,” according to the notice.
https://www.bloomberg.com/news/arti...o-recall-new-wranglers-over-frame-weld-defect